ANSI B16.5-1973、JPI-75-15-70、GB 699、GB1220、JB755、HG20633-9
Mark |
Tolerance(mm) |
P |
±0.177 |
W |
±0.203 |
T |
±0.39 |
Material |
Maximum Hardness |
Temperature( ℃ ) |
Abbreviations |
|
Brinell |
Rockwell“B”Grade |
|||
Soft Iron |
90 |
56 |
-60~500 |
D |
Low Carbon Steel |
120 |
68 |
-40~540 |
S |
SS304 |
160 |
83 |
-250~540 |
304 |
SS304L |
160 |
83 |
-250~540 |
304L |
SS316 |
160 |
83 |
-200~815 |
316 |
SS316L |
160 |
83 |
-200~815 |
316L |
SS321 |
160 |
83 |
-200~870 |
321 |
SS347 |
160 |
83 |
-200~870 |
347 |
SS410 |
170 |
86 |
-40~850 |
410 |
5Cr-0.5Mo |
130 |
|
-29~650 |
|
Copper |
80 |
|
-100~315 |
|
Aluminum |
35 |
|
-200~425 |
|
Inconel 600 |
150 |
|
-100~1095 |
|
Incoloy 825 |
150 |
|
-100~1095 |
|
Monel 400 |
150 |
|
-100~760 |
|
Titanium |
215 |
|
-200~540 |
|
Nickel 200 - |
110 |
|
200~760 |
|
Hastelloy B2 |
230 |
|
-100~1095 |
|
Hastelloy C276 |
210 |
|
-100~1095 |
|